C-Textured Geomembrane

C-Textured Geomembrane

$1.00

Textured HDPE Geomembrane Liner for Enhanced Friction and Slope Stability

✓ High quality & competitive price

✓ Custom sizes and specifications available

✓ Fast delivery worldwide

Product Description

 

Textured HDPE Geomembrane - Premium Liner

Enhanced surface friction with superior mechanical properties for challenging installations

Our Textured HDPE Geomembrane features a specially engineered surface with 0.40mm asperity height, providing exceptional interface friction for slope stabilization. Manufactured with high-density polyethylene, this geomembrane meets rigorous international standards while offering improved installation characteristics.

The textured surface design enhances stability on steep slopes and provides superior bonding with adjacent materials, making it ideal for demanding containment applications where shear resistance is critical.

Textured HDPE Geomembrane Specifications

Properties Unit Inspection Standards C-75 C-100 C-125 C-150 C-200 C-250 C-300 Test Frequency
Thickness mm ASTM D5199 0.75 1.00 1.25 1.50 2.00 2.50 3.00 Per roll
Density g/cc ASTM D1505 / D792 0.94 90,000 kg
Asperity Height - ASTM D7466 0.6–0.7 mm Every 2nd roll
Tensile Properties
Yield Strength
Break Strength
Yield Elongation
Break Elongation
kN/m
kN/m
%
%
ASTM D6693 Type IV 11
18
12
500
15
24
12
500
18
30
12
500
22
36
12
500
29
48
12
500
37
60
12
500
44
72
12
500
9,000 kg
Tear Resistance N ASTM D1004 93 125 156 187 249 311 374 20,000 kg
Puncture Resistance N ASTM D4833 216 288 360 432 576 720 864 20,000 kg
Stress Crack Resistance hr ASTM D5397 ≥500 hr Per GRI GM-10
Carbon Black Content % ASTM D4218 2.0–3.0% 9,000 kg
Carbon Black Dispersion - ASTM D5596 9 of 10 views in Category 1 or 2; 1 in Category 3 20,000 kg
Oxidative Induction Time
(a) Standard OIT
(b) High Pressure OIT
min ASTM D3895 / D5885 100 min / 400 min 90,000 kg
Oven Aging at 85°C – OIT Retention after 90 days
(a) Standard OIT (%)
(b) High Pressure OIT (%)
% ASTM D5721 / D3895 / D5885 55% / 80% Per each formulation
UV Resistance – OIT Retention after 1600 hrs % ASTM D7238 / D5885 50% Per each formulation

Notes:

1. Alternate the measurement side for double sided textured sheet

2. Machine direction (MD) and cross machine direction (XMD) average values should be on the basis of 5 test specimens each direction

3. The SP-NCTL test should be conducted on smooth edges of textured rolls or on smooth sheets made from the same formulation

4. Carbon black dispersion for 10 different views: 9 in Categories 1 or 2 and 1 in Category 3

✅ Key Features:

  • 0.40mm textured surface for superior shear resistance (ASTM D7466)
  • Enhanced thickness tolerance (-5% nominal, -15% maximum)
  • High puncture resistance (200-800N per thickness)
  • Dual OIT protection (Standard 100min or HP-OIT 400min)
  • UV stabilized (≥50% OIT retention after 1600hrs)

✅ Specialized Applications:

  • Steep slope landfill caps (1.5:1 to 1:1 gradients)
  • Mining solution ponds (high friction interface)
  • Reservoir sidewalls (permanent water containment)
  • Wastewater treatment (chemical resistance)
  • Energy sector applications (tailings management)